Haus - Ol Prodak - Blank samting - Ol infomesen
Raw Material bilong Quartz Plate

Raw Material bilong Quartz Plate

Bikpela hat Mohs hat bilong 6~7, wankain olsem 'natural quartz', wantaim strongpela 'wear resistance'.
Heat Resistance Em inap long sanap strong long ol tempereja bilong 150~300 digri (stretpela tolerans i dipen long kain resin).
Korosen Resistens Resistens long ol asid, alkali, na ol kemikel solvent (olsem, alkohol, ol samting bilong klinim).

Diskripsen

Ol bikpela samting

 

Quartz Sand (SiO2): Em i gat 99.99%, na em i strong na i no inap hat.

 

Ol bikpela samting

 

Diskripsen bilong haus

  • Bikpela hat Mohs hat bilong 6~7, wankain olsem 'natural quartz', wantaim strongpela 'wear resistance'.
  • Heat Resistance Em inap long sanap strong long ol tempereja bilong 150~300 digri (stretpela tolerans i dipen long kain resin).
  • Korosen Resistens Resistens long ol asid, alkali, na ol kemikel solvent (olsem, alkohol, ol samting bilong klinim).

 

Ol aplikesen

 

  • Ol Semikondakta Ikwipmen Sabstret:Ol i save yusim ol 'raw material' bilong 'quartz platea' long wokim ol 'chip'.
  • Ol samting bilong pasim hat bilong san:Heat-resistant Raw materiel bilong 'quartz plateserve' olsem 'lining' bilong ol 'kiln' na 'furnace'.

 

Ol propeti

 

  • Petrokemikel indastri
  • Famasiutik indastri
  • Envairomen Enjiniaring

 

Ol propeti

 

Ol samting bilong bodi

Ol veliu

Purity

>99.99%

Mak bilong ol samting i pas pas wantim

2.2g/cm3

Transperensi

>90%

Mohs Hatnes

5.5--6.5

Difomesen Poin

1280 digri

Softening Point

1750 digri

Annealing Point

1250 digri

Spesifik Hat (20 - 350 digri )

670J/kg. digri

Thermal Conductivity (20 degree)

1.4W/m. digri

Heat Conductivity (w/mk,1000 degree)

1.0-1.2

Refraktiv Indeks

1.4585

Koefishen bilong 'Thermal Expansion'

5.510 -7cm/cm. digri

Hot - wok Tempereja

1750--2050 digri

Sotpela - taim Sevis Tempereja

1450 digri

Longpela taim Sevis Tempereja

1100 digri

 

Ol kemikel samting

Ol veliu

No inap long kisim asid

Strongpela Asid (sapos HF i no stap), Strongpela alkali, oganik solusen

Ol bikpela hat i no inap bagarap

Nambawan

Metal Impuriti Konten

<5 ppm

 

Ol samting bilong pawa

Ol veliu

Resistiviti

7107Ω.cm

Strong bilong insulesen

250~400Kv/cm

Dielectric Constant

3.7~3.9

Dielectric Absorption Coefficient

<410-4

Dielectric Loss Coefficient

<110-4

 

Ol samting bilong masin

Ol veliu

Strong bilong presim

1100MPa

Strong bilong bendim

67MPa

Strong bilong 'Tensile'

48MPa

Poisson's Ratio

0.14~0.17

Young's Modulus

72000MPa

Shear Modulus

31000MPa